Heat Exchanger Tube Inspection and Leak Testing Methods Explained

Heat exchanger tube inspection explained: eddy current vs IRIS, remote field testing, hydrotests and leak tests, and how plugging and retube decisions are made.

By Syed Hasan26 Nov 20269 min read

Heat Exchanger Tube Inspection and Leak Testing Methods Explained

The bundle is out, cleaned and sitting on the pad. You have a few days of the turnaround to decide whether it goes back in as it is, goes back with some tubes plugged, or gets retubed. Hundreds of tubes, each one hidden inside the next row, and the only clue to their condition is what your inspection methods can tell you.

This post walks through heat exchanger tube inspection and leak testing as they are actually done: visual and borescope checks, eddy current, IRIS and the related electromagnetic methods, hydrotests and other leak tests, and the plugging and retubing decisions that follow. For each method you get what it finds, what it misses and when to use it, so you can read an inspection report and judge whether it answered the question you needed answered.

Start with your eyes: visual and borescope inspection

Every heat exchanger tube inspection starts with a look. On the tubesheet face, check the tube ends for thinning, erosion at the inlet, cracking at the rolled or welded joint, and corrosion of the tubesheet ligaments between holes. On a pulled bundle, look along the outer rows for deposits, wear marks at the baffles and damage from shell-side flow at the inlet nozzle. The names of each part, and where they sit, are set out in inside a shell and tube heat exchanger.

A borescope or video probe lets you see a short way inside individual tubes. It is good for confirming pitting, deposits or a blockage that another method flagged, but it shows the surface only, not the wall thickness behind it.

None of the methods below work well on a dirty tube. Deposits block probes, scatter signals and hide the surface. Cleaning is part of the inspection, and the reasons deposits form are covered in fouling in heat exchangers.

Eddy current testing: the fast screening method

In eddy current testing, heat exchanger tubes are scanned one at a time with a probe, usually a bobbin coil, pushed through each tube. An alternating current in the coil induces small electrical currents in the tube wall. Wall loss, pits and some cracks disturb those currents, and the instrument records the change as the probe is pulled back out.

Its strength is speed. A trained crew can test a large number of tubes in a shift, which is why it is the usual first choice for screening a whole bundle. Results are calibrated against a reference tube of the same material and size with machined defects of known depth, so the analyst can estimate how deep an indication is.

The main limit is the material. Conventional eddy current works on non-ferromagnetic tubes: austenitic stainless steel, copper alloys, titanium and nickel alloys. Carbon steel and other ferromagnetic tubes need a different electromagnetic method, covered below. Sizing small, sharp pits is also less certain than sizing general wall loss, and the readings near the tubesheet and at support plates need careful interpretation.

Photograph of a technician feeding an eddy current bobbin probe into a tube at the tubesheet face of a cleaned heat exchanger bundle
Eddy current screening: a bobbin probe is pushed through each tube and pulled back.

IRIS: measuring the wall directly

IRIS stands for internal rotary inspection system. It is an ultrasonic method: a transducer fires sound at a rotating mirror inside the tube, which sweeps the beam around the full circumference as the probe is pulled along. The tube is flooded with water to carry the sound. The result is a direct measurement of wall thickness all the way round, displayed as a map of each tube.

Because it measures thickness rather than inferring it, IRIS tube inspection is often used to confirm and size what a faster screening method found, and it works on ferromagnetic and non-ferromagnetic tubes alike. The trade-offs are that it is slow, it needs very clean tubes, and it is not the method of choice for finding cracks.

Heat exchanger tube inspection: eddy current or IRIS?

PointEddy currentIRIS
How it worksInduced currents in the tube wallUltrasound swept round the tube by a rotating mirror
Tube materialsNon-ferromagnetic tubesFerromagnetic and non-ferromagnetic
SpeedFast, suited to whole bundlesSlow, suited to selected tubes
Wall readingEstimated from calibrationMeasured directly, full circumference
Cleanliness neededClean boreVery clean bore, tube flooded with water
Typical useScreening the bundleConfirming and sizing indications

In practice the two are often combined: screen the bundle with a fast electromagnetic method, then use IRIS on the tubes that showed the worst indications and on a sample of the rest. That gives coverage and accurate sizing without spending days on one exchanger.

Diagram of an IRIS probe inside a water-filled tube, with a rotating mirror sweeping an ultrasonic beam around the wall and a wall thickness map beside it
IRIS sweeps an ultrasonic beam round the tube and maps the wall thickness.

Carbon steel tubes: remote field and related methods

Ferromagnetic tubes defeat conventional eddy current because the steel's magnetic properties swamp the signal. Remote field testing uses a lower frequency and a receiver set some distance from the exciter coil, and it can screen carbon steel tubes for wall loss. Near field testing is used for finned carbon steel tubes, such as those in air coolers, where the fins make other methods difficult. Magnetic flux leakage probes are another option for detecting localised metal loss in ferromagnetic tubes.

These methods are good at telling you that wall loss is present and roughly where. Where an accurate depth is needed, the indication is usually confirmed with IRIS.

Leak testing: finding the tube that is already through

Inspection methods tell you about wall loss before a leak. Heat exchanger leak testing tells you which tubes or joints are already leaking, which is often the first question when an exchanger is taken offline with contaminated product or cooling water.

Shell-side hydrotest. With the channel cover or head removed, the shell side is filled with water and pressurised. Any tube or tube-to-tubesheet joint that leaks shows as water at the tubesheet face, so the inspector can see exactly which hole it is coming from. A floating-head exchanger needs a test ring to seal the floating end so the tubesheet can be observed. The test pressure comes from the design code and the owner's procedure, not from a rule of thumb.

Tube-side test. Pressurising the tube side and watching the shell side shows whether a leak exists, but not which tube it is in, so it is used to confirm integrity rather than to locate a defect.

Individual tube tests. Single tubes can be checked by pressurising or applying vacuum to each one with a test gun or plugs and watching for pressure decay. Tracer gas methods, such as helium leak testing, are used where very small leaks matter. These let you separate a tube leak from a joint leak, which matters because a leaking rolled joint can often be re-rolled, while a holed tube cannot be repaired in place.

Diagram of a shell-side hydrotest with the channel removed, water under pressure on the shell side and a leaking tube end visible at the tubesheet
A shell-side hydrotest shows exactly which tube or joint is leaking.

Plugging, sleeving or retubing

Once the leaks and the worst tubes are known, the decisions follow. A tube that is leaking or whose wall loss exceeds the owner's acceptance criteria is usually plugged at both ends. Tubes next to a failed one are often checked closely, and sometimes plugged as well, because the cause that holed one tube is likely acting on its neighbours.

Tube plugging takes heat transfer area out of service and raises the velocity in the remaining tubes. Every exchanger therefore has a point where plugging more tubes would leave it unable to do its duty, and that point comes from its thermal design margin and the owner's specification, not from a general figure. Track the number and position of plugged tubes on a tubesheet map at every turnaround, because the pattern shows where damage is concentrated. How much margin a given exchanger has depends on its duty, which is why the same plugging count can be harmless on one service and critical on another; the main exchanger duties in plants are described in heat exchangers in oil and gas.

Retubing becomes the better choice when damage is widespread, when the plugged count is close to the thermal limit, or when inspection shows the whole bundle thinning at a rate that will not last another run. Where the damage is local to the tube ends, inserts or sleeves can sometimes extend life without retubing. A sound remaining life estimate, based on wall readings from successive inspections, is what turns this from a guess into a decision.

Frequently asked questions

What methods are used for heat exchanger tube inspection?

The usual set is visual and borescope checks, eddy current for screening non-ferromagnetic tubes, IRIS for direct wall thickness, and remote field, near field or magnetic flux leakage probes for carbon steel tubes. Leak tests, such as a shell-side hydrotest or individual tube tests, then find the tubes or joints already leaking.

Can eddy current be used on carbon steel tubes?

Not conventional eddy current, because the steel's magnetic properties swamp the signal. Remote field testing uses a lower frequency and a receiver set away from the exciter coil to screen carbon steel tubes for wall loss, near field testing suits finned tubes, and any indication that needs an accurate depth is usually confirmed with IRIS.

What is the difference between eddy current and IRIS?

Eddy current is fast and suited to screening a whole bundle, but it works on non-ferromagnetic tubes and estimates depth from calibration. IRIS is slow and needs very clean, water-filled tubes, but it measures wall thickness directly around the full circumference on any tube material, so it is used to confirm and size indications.

How do you find which tube is leaking?

Remove the channel cover or head, fill the shell side with water and pressurise it, then watch the tubesheet face; water shows at the leaking tube or joint. A floating-head exchanger needs a test ring. Individual tube tests with a test gun, or helium leak testing for very small leaks, separate a tube leak from a joint leak.

What to do next

Before the next turnaround, write down what question each method is meant to answer for each exchanger: screening, sizing, locating a leak or confirming the joints. Then choose the methods to suit the tube material and the damage you expect, and agree the acceptance criteria and plugging limit before the bundle comes out, not while it sits on the pad. The heat exchanger inspection and maintenance course covers these methods in practice, and the heat exchanger integrity and tube bundle assessment programme goes further into damage mechanisms, remaining life and retube decisions.

Exam preparation

Preparing for API 510?

Practise with exam-style questions, timed mocks and study notes. 2,549 questions in the bank.

  • Heat exchangers
  • NDT
  • Eddy current
  • IRIS
  • Leak testing
  • +2
Share

Related Certifications

Certifications covered in this article. Each guide has the exam format, eligibility route and a practice question bank.