Welcome to Excellence Integrity Management - Empowering Professionals Globally.
Toolkit

Naphthenic Acid Corrosion (NAC)

API 571 section 3.46. Summary for learning.

Follows API 571 terminology

What is it
High-temperature (425–750°F), hot-DRY-hydrocarbon attack by organic naphthenic acids in crude — velocity-sensitive grooving/pitting governed by TAN, sulfur content, and molybdenum alloying, with whole-crude TAN a notoriously poor predictor.
What is the critical factor
NAC is a function of naphthenic acid content, temperature, sulfur content, velocity (WALL SHEAR STRESS), and alloy composition. Severity increases with increasing acidity of the hydrocarbon phase.
Which materials are affected
Carbon steel, low-alloy steels, 400-series SS, 300-series SS, and nickel-based alloys.
How is it prevented or mitigated
For systems not designed for NAC: change or BLEND crudes (reduce TAN and/or increase sulfur), upgrade alloy, use chemical inhibitors — or combinations.
What is the exam focus point
Temperature window: primarily 425–750°F (220–400°C); reported as low as 350°F; coker gas oil cases to 800°F.

Summaries for learning, based on API 571. The standard and your corrosion-control documents govern.

Preparing for API 571? See the exam preparation

Preparing for an exam? Take it with you.

The EIM app has study notes, practice questions with explanations, timed mock tests and your progress, on your phone. Free to download. Android first, iPhone to follow.