Welcome to Excellence Integrity Management - Empowering Professionals Globally.
Toolkit

Amine Corrosion

API 571 section 3.2. Summary for learning.

Follows API 571 terminology

What is it
Localized carbon steel attack in amine treating units caused NOT by the amine itself but by dissolved acid gases (CO2/H2S), heat-stable amine salts, and degradation products — governed by amine type (MEA worst, MDEA mildest), velocity limits (3–6 fps rich, ~20 fps lean), and the 220°F flashing threshold.
What is the critical factor
Design and operating practices, TYPE of amine, contaminants, temperature, and velocity.
Which materials are affected
Primarily carbon steel. 300-series SS and other stainless grades are more resistant.
How is it prevented or mitigated
PROPER OPERATION is the most effective control: watch acid gas loading; keep process temperature within limits to avoid corrosive degradation products; control reboiler rate and temperature to hold regenerator temperatures.
What is the exam focus point
'Not the amine, but the acid gases' — the definitional trap: CO2/H2S, HSAS, and degradation products (bicine/oxalate/formate) do the damage.

Summaries for learning, based on API 571. The standard and your corrosion-control documents govern.

Preparing for API 571? See the exam preparation

Preparing for an exam? Take it with you.

The EIM app has study notes, practice questions with explanations, timed mock tests and your progress, on your phone. Free to download. Android first, iPhone to follow.

Get it on Google Play