Welcome to Excellence Integrity Management - Empowering Professionals Globally.
Toolkit

Sulfidation (Sulfidic Corrosion)

API 571 section 3.61. Summary for learning.

Follows API 571 terminology

What is it
High-temperature reaction of steel with sulfur compounds WITHOUT hydrogen present — practical concern above 500°F, governed by chromium content and 'reactive sulfur', famous for uniform thinning that ends in RUPTURE and for the low-silicon carbon steel trap. API RP 939-C governs.
What is the critical factor
Major factors: metal chemical composition, temperature, and concentration of corrosive (REACTIVE) sulfur compounds. Flow conditions also affect the rate.
Which materials are affected
All iron-based materials, in order from MOST to LESS susceptible: carbon steel and low-alloy steels → 400-series SS → 300-series SS.
How is it prevented or mitigated
Upgrade to higher-chromium steel — 9Cr-1Mo is the standard escalation.
What is the exam focus point
The temperature pair: begins >450°F (230°C), practical concern >500°F (260°C) — 500°F is the inspection-focus threshold.

Summaries for learning, based on API 571. The standard and your corrosion-control documents govern.