Tank bottoms corrode from both sides. The soil side suffers from moisture, poor drainage, stray current and no cathodic protection. The product side suffers from water, sludge and microbial attack that pit the floor. Pitting is localised and easy to miss.
- Soil-side corrosion comes from moisture, aggressive fill, poor drainage, stray currents and missing cathodic protection.
- Product-side corrosion comes from water that settles on the floor, sludge, acids and microbial growth.
- Corrosion on a bottom is often pitting, not even thinning, so an average reading can hide a deep pit.
- The edge of the bottom, near the shell, is a common place for trouble.
Tank bottoms are a leading concern in tank integrity because they corrode from both sides and are hard to examine. A leak through the floor goes into the ground, where it may go unnoticed for a long time.
On the soil side, the steel is in contact with the foundation. Moisture, salts in the fill, poor drainage and ground that holds water all make corrosion more likely. Stray electrical currents can speed it up. Without cathodic protection, a bottom on wet or aggressive ground can lose metal steadily. Where the bottom is supported by a ring wall, water can collect at the edge and attack the annular plates.
On the product side, the usual culprit is water. Water is heavier than most stored products and settles at the bottom, along with sludge and solids. Under the sludge, bacteria can thrive and create local acid conditions that pit the steel. Some products carry acids or sulfur compounds that add to the problem.
What makes bottom corrosion tricky is that it tends to be local. A floor may be sound over most of its area and have a few deep pits that control the remaining life. That is why inspectors scan the floor with tools that map metal loss over a wide area, then follow up with direct measurement of the worst pits, rather than rely on a handful of spot readings.
Protection comes from good foundation design and drainage, cathodic protection, linings on the inside of the bottom, regular water draw-off and cleaning, and inspection at an interval that matches how fast the floor is actually corroding.
Good practice
- Plan floor scanning and pit depth measurement when the tank is out of service.
- Look for a pattern: pits near the centre, along weld seams, or at the edge tell different stories.
Avoid
- Do not judge a floor from a few thickness readings.
- Do not ignore the underside because the top surface looks clean.
In the field
Where water has been draining out of a tank for years, expect corrosion under the sump and along the lowest plates. Start your scan there.
- Soil-side corrosion:
- attack on the underside of the bottom by the ground.
- Pitting:
- deep, localised corrosion in small areas.
- MIC:
- microbiologically influenced corrosion, caused or accelerated by bacteria.
Based on: API 653, API 651, API 652. A summary for learning. The standard and your site procedures govern.
Preparing for an exam? Take it with you.
The EIM app has study notes, practice questions with explanations, timed mock tests and your progress, on your phone. Free to download. Android first, iPhone to follow.