Welcome to Excellence Integrity Management - Empowering Professionals Globally.
Toolkit

High-Temperature Hydrogen Attack (HTHA)

API 571 section 3.36. Summary for learning.

Follows API 571 terminology

What is it
Reaction of atomic hydrogen with carbides in steel above ~400–600°F to form methane — causing surface/internal decarburization, then intergranular fissuring and cracking. Governed by the API RP 941 Nelson curves, with an unpredictable INCUBATION period, irreversible cumulative damage, and the removal of the C-½Mo curve in 1990.
What is the critical factor
Resistance increases with alloy content (primarily Cr and Mo). For a given material, HTHA depends on temperature, hydrogen PARTIAL PRESSURE, time, and stress level.
Which materials are affected
In order of INCREASING resistance: as-welded (non-PWHT) carbon steel; non-welded / PWHT'd carbon steel; C-0.5Mo; Mn-0.5Mo; 1Cr-0.5Mo; 1.25Cr-0.5Mo; 2.25Cr-1Mo; 2.25Cr-1Mo-V; 3Cr-1Mo; 5Cr-0.5Mo; and similar.
How is it prevented or mitigated
Use Cr-Mo alloy steels for carbide stability (also W and V stabilize carbides), minimizing CH4 formation.
What is the exam focus point
The mechanism: atomic H + carbides → CH4 (methane) that can't diffuse out → cavities → fissures → intergranular cracks adjacent to PEARLITE.

Summaries for learning, based on API 571. The standard and your corrosion-control documents govern.

Preparing for API 571? See the exam preparation

Preparing for an exam? Take it with you.

The EIM app has study notes, practice questions with explanations, timed mock tests and your progress, on your phone. Free to download. Android first, iPhone to follow.